Home | Site Contents | Search | aluSelect | Partners |About aluMATTER | Help  
Click here to go to the top-level of the aluMATTER site blank spacer  
Page 1 / 1  
aluMATTER logo lower section  
Select Language:

Send Feedback to EAA

Leonardo da Vinci, Helsinki Award 2006, Design and execution: Gerold Fink, Austria. Click to open PDF document about this award

Leonardo Da Vinci Helsinki Award 2006

Leonardo da Vinci, Helsinki Award 2006, Design and execution: Gerold Fink, Austria. Click to open PDF document about this award

Bronze medal for an outstanding project promoting and supporting the LifeLong Learning EU policy. Award Berlin 2007

 
Casting Alloys Classifications

Casting alloys are classified by composition using a 3.1 digit number.

The first digit specifies the major alloying element(s)

1xx.x 99.00 wt% min. aluminium  
2xx.x Al-Cu See phase diagram
3xx.x Al-Si-(Cu/Mg) See phase diagram (Al-Si)
4xx.x Al-Si See phase diagram
5xx.x Al-Mg See phase diagram
6xx.x Unused series  
7xx.x Al-Zn See phase diagram
8xx.x Al-Sn  
9xx.x Others  