Microstructural Development

Leonardo da Vinci, Helsinki Award 2006, Design and execution: Gerold Fink, Austria. Click to open PDF document about this award

Leonardo Da Vinci Helsinki Award 2006

Leonardo da Vinci, Helsinki Award 2006, Design and execution: Gerold Fink, Austria. Click to open PDF document about this award

Bronze medal for an outstanding project promoting and supporting the LifeLong Learning EU policy. Award Berlin 2007

 
Click to go to the previous page in this section Page 9 / 17 Click to go to the next page in this section  
Precipitation in Al-Cu
Click to view larger image
blank spacer
Click to view larger image
Micrograph showing Cu rich GP zones in Al-4%Cu, aged for 6 hours at 180 °C.
Courtesy of MH Jacobs, The University of Birmingham.
 
Micrograph showing θ' precipitates in Al-4%Cu, aged for 2 hours at 200 °C.
Courtesy of MH Jacobs, The University of Birmingham.
 
Click to view larger image
Micrograph showing θ precipitates in Al-4%Cu, aged for 45 mins at 450 °C.
Courtesy of MH Jacobs, The University of Birmingham.

 

 

See Also

External Links

EAA, MATTER and their partners are not responsible for the content of external sites.

References

  • MATTER Project, "Materials Science on CD-ROM", Chapman & Hall, 0412836602
  • Porter DA and Easterling KE, "Phase transformations in metals and alloys", Chapman & Hall, 0412450305

Full details here...

Authors/Contributors