...by tailoring the surface of aluminium sheet, various
optical effects can be generated. Have you ever wondered why your aluminium
thermos is so reflective, while your aluminium door has a matt appearance?
...several solutions have been developed to improve adhesion of coatings
and organic films on aluminium. This adhesion ensures, for example, a
lifespan of over 25 years for coated aluminium window frames.