Go to the aluSelect Home Page Alloys Available by Product Form
Wrought Alloys
------------------
Casting Alloys

Go to aluMATTER Website...

The following alloys are available in "Profile section shape" form:

1050A  1200  2014  2014A  2017A  2024  3003  3103  5005  5005A  5049  5052  5083  5086  5154A  5251  5454  5754  6005A  6060  6061  6063  6082  6106  7020  7075