ALLOY AA ASTM BS BS(OLD) DIN INTER ISO JIS JIS(OLD) NF NF(OLD) SFS SNCH SS UNI UNI(OLD) UNS WNR NS UNE ASV ALUSUISSE CSA(OLD) GOST(OLD) ALCAN VAW_L STDREF
    USA GB GB Germany   Intl. Japan Japan France France Finland Switz. Sweden Italy Italy   Germany                  
1050A (1050) (1050) 1050A 1B Al99,5 1050A Al99,5 (A1050) A1x1 1050A A5 2582 Al99,5 4007 9001/2 4507 (A91050) 3.0255 17010 L-3051 1005 1500 9950 A5/ADO 1S 99/50 ALSCHL87
1200 1200   1200 1C Al99 1200 Al99,0 A1200 A1x3 1200 A4 2584 Al99 4010 9001/1 3567   3.0205 17005 L-3001 1008 1100 990 A/A0 2S 99/00 ALSCHL87
2007 2007       AlCuMgPb 2007 (Al Cu4PbMg)       (A-U4Pb)   AlCu4MgPb 4335 9002/8     3.1645   L-3121   2118       18/00 ALSCHL87
2011 2011 2011 2011 FC1 AlCuBiPb 2011 Al Cu6BiPb A2011   2011 A-U5PbBi   (AlCu6BiPb) 4355 9002/5 6362 A92011 3.1655   L-3192   2500 CB60   28S 14/11 ALSCHL87
2014 2014 2014 (2014A) (H15) AlCuSiMn 2014 Al Cu4SiMg A2014 A3x1 2014 A-U4SG 2595 AlCu4SiMn 4338 9002/3 3581 A92014 3.1255 17105 L-3130   2662 CS41N AK8 26S 17/41 ALSCHL87
2014A (2014)   2014A H15 (AlCuSiMn) 2014A Al Cu4SiMg(A)       (A-U4SG) (2595)   (4338)   3501   (3.1255)                  
2017A (2017) (2017) 2017A   AlCuMg1 2017A Al Cu4MgSi(A) (A2017) A3x2 2017A A-U4G       9002/2 3579 (A92017) 3.1325   L-3120   2100 CM41 D1/V65 17S 17/69 ALSCHL87
2024 2024 2024 2024 2L97 AlCuMg2 2024 Al Cu4Mg1 A2024 A3x4 2024 A-U4G1   AlCu4Mg1,5   9002/4 3583 A92024 3.1355   L-3140   2150 CG42 D16 24S 17/24 ALSCHL87
2030 2030       (AlCuMgPb) 2030 Al Cu4PbMg     2030 A-U4Pb   (AlCu4MgPb)         (3.1645)                  
3003 3003 3003 (3103)   AlMnCu 3003 Al Mn1Cu A3003 A2x3 3003 A-M1       9003/1 7788 A93003 3.0517   L-3810 2030 3103 MC10 AMc D3S 41/20 ALSCHL87
3004 3004       Al Mn1Mg1   Al Mn1Mg1       A-MG1         6361       L-3820         D4S, 4S 61/03  
3005 3005       Al Mn1Mg0,5   Al Mn1Mg0,5       A-MG0,5                           C4S 61/16  
3103 3103   3103 N3 AlMn1 3103 Al Mn1         2585 AlMn 4054 9003/3 3568   3.0515 17405 L-3811 2029 3100 M1 (AMc) 3S 41/00 ALSCHL87
3105 3105       Al Mn0,5Mg0,5   Al Mn0,5Mg0,5                                        
5005 5005 5005 5005 N41 (AlMg1) 5005 Al Mg1(B) A5005   5005 A-G0.6 2586   4106 9005/1 5764 A95005 (3.3315)                  
5005A (5005)   (5005) N41 AlMg1 5005A     A2x8   (A-G0.6)   AlMg1 (4106)   (5764)   3.3315   L-3350   5100   AlMg1 B57S 63/10 ALSCHL87
5049 5049       Al Mg2Mn0,8   Al Mg2Mn0,8                                   B4S 61/40  
5052 5052 5052     AlMg2,5 5052 Al Mg2,5 A5052 A2x1 5052 A-G2.5C 2587 AlMg2,5 4120 9005/2 3574   3.3523 17210 L-3360 2041 5253 GR20   57S 63/52 ALSCHL87
5083 5083 5083 5083 N8 AlMg4,5Mn 5083 Al Mg4,5Mn0,7 A5083 A2x7 5083 A-G4.5MC   AlMg4,5Mn 4140 9005/5 7790 A95083 3.3547 17215 L-3321 2021 5460 GM41   D54S 61/83 ALSCHL87
5086 5086 5086     AlMg4Mn 5086 Al Mg4 A5086   5086 A-G4MC   AlMg4Mn   9005/4 5452 A95086 3.3545   L-3322 2028 5410   AMg4 E54S 63/40 ALSCHL87
5154A (5154)   5154A N5   5154A Al Mg3,5(A) (A5154)             (9005/8) 3575                      
5182 5182       Al Mg5Mn   Al Mg4,5Mn0,4                                   A56S 63/65  
5251 5251   5251 N4 AlMg2Mn0,3 5251 Al Mg2     5251 A-G2M             3.3525 17205 L-3361 2023 5200   AMg2 M57S 63/21 ALSCHL87
5454 5454 5454 5454 N51 AlMg2,7Mn 5454 Al Mg3Mn A5454 A2x9 5454 A-G2.5MC   AlMg2,7Mn   9005/3 7789 A95454 3.3537   L-3391 2078 5260 GM31N   B53S 61/54 ALSCHL87
5754 5754       AlMg3 5754 Al Mg3     5754 A-G3M 2588 AlMg3 4125       3.3535   L-3390 2014 5300   AMg3 53S 63/30 ALSCHL87
6005A (6005)       AlMgSi0,7 6005A Al SiMg(A) (A6NO1)   6005A A-GS0.5   AlMgSi0,7   9006/6     3.3210   L-3454   6062     C51S 19/23 ALSCHL87
6016 6016                                                    
6060 6060 (6063) (6063) (H9) AlMgSi0,5 6060 Al MgSi (A6063) A2x5 6060 A-GS   AlMgSi0,5 4103 9006/1 3569 (A96063) 3.3206 17310 L-3441 2032 6050 GS10 (AD31) G50S,50S 19/07 ALSCHL87
6061 6061 6061 6061 H20 AlMg1SiCu 6061 Al Mg1SiCu A6061 A2x4 6061 A-GSUC       9006/2 6170 A96061 3.3211   L-3420 2079 (6061) GS11N AD33/AV 65S,C65S 19/61 ALSCHL87
6063 6063 6063 6063 H9 (AlMgSi0,5) 6063 Al Mg0,7Si A6063 A2x5   (A-GS) 2591   4104   (3569)   (3.3206) 17310 L-3441 2032 6050 GS10 (AD31) G50S,50S 19/07 ALSCHL87
6082 6082   6082 H30 AlMgSi1 6082 Al Si1MgMn     6082 A-GSM0.7 2593 AlMgSi1Mn 4212 (9006/4) 3571   3.2315 17305 L-3451 2005 6112 SG11R AD35 B51S 19/45 ALSCHL87
6106 6106           Al MgSiMn                                        
7010 7010   7010 DTD5130   7010 Al Zn6MgCu               9007/4                        
7020 7020 (7005) 7020 H17 AlZn4,5Mg1 7020 Al Zn4,5Mg1 (A7N01)   7020 A-Z5G 2596 AlZn4,5Mg1 4425 9007/1 7791 (A97005) 3.4335 17410 L-3741   7100   (1915) D74S 21/51 ALSCHL87
7075 7075 7075 7075 2L95 AlZnMgCu1,5 7075 Al Zn5,5MgCu A7075 A34x6 7075 A-Z5GU   AlZn6MgCu1,5   9007/2 3735 A97075 3.4365   L-3710 2082 7215 ZG62 B95(V95) 75S 20/75 ALSCHL87