Wrought Alloys
------------------ Casting
Alloys
|
 |
As fabricated. Shaped by cold working, hot working or casting processes in which no special control over thermal conditions or strain hardening is employed.
|
|
 |
Full tempers:
| F |
As fabricated. Shaped by cold working, hot working or casting processes in which no special control over thermal processes or strain hardening is employed. |
|
|
 |