Go to the aluSelect Home Page Cast Alloys: Physical and Surface Properties
Wrought Alloys
------------------
Casting Alloys

Go to aluMATTER Website...

Alloys:

EN AC-42000
Chemical designator
a
l
EC
Fluidity
HBN
Decor Anod
Weldability
Corrosion
µm m-1 K-1
W m-1 K-1
%IACS
       
EN AC-AlSi7Mg
22
150-170
33-43
6
5
4
6
5-6
 

 

 
Key to Parameters: Key to Values:
a Coefficient of thermal expansion  µm m-1 K-1
l: Thermal conductivity W m-1 K-1
EC: Electrical conductivity %IACS
Fluidity: Fluidity 2-7
HBN: Polishing ability 2-7
Decor Anod:  Decorative anodizing 2-7
Weldability:  Weldability 2-7
Corrosion: Corrosion 2-7
 
-:  No information available  
1:  Not applicable  
2:  Unsuitable  
3:  Not recommended  
4:  Acceptable  
5:  Good  
5-6:  Good to Very Good  
6:  Very Good  
7:  Excellent