Go to the aluSelect Home Page Casting Alloys: Mechanical Properties
Wrought Alloys
------------------
Casting Alloys

Go to aluMATTER Website...

Alloys:

Methods:

Please select alloy and casting method from menus on the left.  
Key to Properties Key to Values:
  Min 0.2% Proof Stress
MPa
  Min UTS MPa
  Elongation A50 %
HB:   Hardness, Brinell HB
  Fatigue Endurance Limit 107 cycles   
  Hot tear resistance scale 2-7
  Machinability scale 2-7
  Pressure Tightness scale 2-7
 
-:  No information available  
1:  Not applicable  
2:  Unsuitable  
3:  Not recommended  
4:  Acceptable  
5:  Good  
5-6:  Good to Very Good  
6:  Very Good  
7:  Excellent