EN AW-2024
Cu 3.8 - 4.9
Mg 1.2 - 1.8
Mn 0.30 - 0.9
Fe <= 0.50
Si <= 0.50
Zn <= 0.25
Zr+Ti <= 0.20
Total Other <= 0.15
Ti <= 0.15
Cr <= 0.10
Other Elem <= 0.05
Al Remainder

All compositions in wt%.


 

 